b) Ferrite: Solid solution of carbon in BCC iron from room temperature to 910 deg.C Max solubility of C is .. 0.022% at temp. of 727 deg.c Also called as Alpha Ferrite. Softest phase in Fe-Fe3C phase diagram.. less strength and High ductility Cementite: Intermetallic compound of Carbon combined with Iron..Fe3C Max solubility of Carbon is of 6.67%. Orthorhombic crystal structure
Hardest and most brittle phase among all Fe-Fe3C phases. Austenite: Solid solution of Carbon in FCC iron..Also called as Gamma Iron. Exists from 910–1395 deg.C Max solubility of Carbon .. 2.11% at 1147 deg.C Toughest phase among all... Strength along with optimum Ductility Pearlite: Mixture of Ferrite and Cementite (alternately arranged as like pearls) we can find 100% pearlite at 727 deg.C. Soft Phase than Austenite but posses better strength than Ferrite.